Kompomer restorasyon materyallerinin süt dişlerinde kullanılabilirliğinin in-vivo ve in-vitro değerlendirilmesi

Evoluation of compomer restoration materials on decidious dentition - An In vivo and in vitro study

  1. Tez No: 71093
  2. Yazar: SİBEL BURMABIYIKOĞLU
  3. Danışmanlar: PROF. DR. ZEYNEP AYTEPE
  4. Tez Türü: Doktora
  5. Konular: Diş Hekimliği, Dentistry
  6. Anahtar Kelimeler: Cam iyonomer çimentoları, Dental materyaller, Kök kanal dolgu materyalleri, Süt dişleri, Glass ionomer cements, Dental materials, Root canal filling materials, Tooth deciduous
  7. Yıl: 1997
  8. Dil: Türkçe
  9. Üniversite: İstanbul Üniversitesi
  10. Enstitü: Sağlık Bilimleri Enstitüsü
  11. Ana Bilim Dalı: Pedodonti Ana Bilim Dalı
  12. Bilim Dalı: Belirtilmemiş.
  13. Sayfa Sayısı: Belirtilmemiş.

Özet

110 ÖZET Bu araştırmada, kompomer restorasyon materyallerinin (Compoglass ve Dyract) klinik özellikleri ve kenar sızıntısı in-vivo olarak, yüzey sertliği ve aşınmaya karşı dirençler in-vitro olarak, hibrid kompozit reçine (TPH Spect rum) ve geleneksel cam iyonomer siman (lonofil U) ile karşılaştırmalı olarak incelenmiştir. Dört çalışmadan oluşan bu araştırmanın birinci çalışmasında yaşları 8-10 arasında değişen 19 hastanın 76 adet çürüksüz süt azı dişine, 19'lu gruplar halinde Compoglass ve Dyract kompomer restorasyon materyalleri, TPH Spectrum hibrid kompozit reçine ve lonofil U geleneksel cam iyonomer siman ile restorasyon yapılmıştır. Hastalar 3. ve 6. ayda klinik kontrollere alınarak, USPHS sistemine göre, restorasyonların renk uyumu, yüzey kenarı renkleşmesi, anatomik şekil, kenar uyumu ve sekonder çürük oluşumu ile ilgili özellikleri değerlendirilmiştir. Compoglass kompomer materyalinin kenar uyumu, Dyract kompo mer materyalinin renk uyumu, yüzey kenarı renkleşmesi ve anatomik şekille ilgili özelliklerinin daha başarılı olduğu gözlenmiştir. Yüzey kenarı renkleşme si ile ilgili değerlendirmede lonofil U daha düşük kabul edilebilirlik oranı göstermiştir ve hiç bir restorasyonda sekonder çürük oluşumu gözlenmemiştir. 6 aylık klinik değerlendirme sonucunda, süt azı dişlerindeki kompo mer, hibrid kompozit reçine ve geleneksel cam iyonomer siman restorasyonları arasında anlamlı bir farklılık bulunmamıştır. İkinci çalışmada Compoglass ve Dyract kompomer restorasyon materyalleri, TPH Spectrum hibrid kompozit reçine ve lonofil U geleneksel cam iyonomer siman ile yapılan restorasyonlar kenar sızıntısı açısından incelen miştir.111 52 adet süt azı dişi, restorasyon yapımını izleyen 6. ayın sonunda çekilmiş ve kesit alınarak metilen mavisi boyama yöntemi ile ışık mikroskobunda incelenmişlerdir. Kompomer, hibrid kompozit reçine ve geleneksel cam iyonomer restorasyonların kenar sızıntısı değerleri arasında anlamlı bir farklılık bulunmamıştır. Üçüncü çalışmada her grupta 8'er adet olacak şekilde hazırlanan örneklerde, 4 grup restorasyon materyalinin yüzey sertlikleri in-vitro koşullarda Vickers Sertlik Apareyi ile incelenmiştir. Compoglass ve Dyract kompomer restorasyon materyalleri arasında anlamlı bir farklılık bulunmadığı, TPH Spectrum hibrid kompozit materyalin yüzey sertliğinin diğer 3 restorasyon materyaline oranla anlamlı derecede yüksek olduğu saptanmıştır, lonofil U geleneksel cam iyonomer simanın yüzey sertlerinin ise 14. günden sonra kompomer restorasyon materyallerin yüzey sertliğinden anlamlı derecede daha yüksek olduğu gözlenmiştir. Dördüncü çalışmada her grupta 6'şar adet olacak şekilde hazırlanan örneklerde 4 grup restorasyon materyalinin aşındırma apareyi ile gösterdikleri aşınmalar arasında anlamlı farklılık bulunmamıştır. Sonuç olarak, kompomer restorasyon materyallerinin süt dişlerinin restorasyonları için uygun niteliklere sahip materyaller olabileceği görüşüne varılmıştır.

Özet (Çeviri)

112 SUMMARY in this study, the clinical assessment, marginal leakage, wear and microhardness of compomer restorative materials (Compoglass and Dyract) were investigated comparatively with a traditional glass ionomer cement (lonofil U) and a hybrid composite resin (TPH Spectrum). This study consist of 4 parts. in the first part, 19 children aged betvveen 8-10 years volunteered. 76 caries-free primary molars were divided into 4 groups, each consisting of 19 teeth and they were restored with compomer restorative materials (Compoglass and Dyract), a hybrid composite resin (TPH Spectrum) and a traditional glass ionomer cement (lonofil U). The clinical evaluation of the restorations were assessed during a 3 and 6 month follow-up period. The color match, cavosurface discoloration, anatomical form, marginal adaptation and secondary caries formation of restorations were evaluated using USPHS criteria. Although Compoglass compomer material shovved good marginal adaptation than the other restorative materials, Dyract restorations appeared with good color match, cavosurface discoloration. The evaluation of cavosurface discoloration lonofil U restorations were found clinically acceptable and there were no secondary caries formation in ali of the 4 groups. There was no statistically significant difference in the clinical evaluation of the compomer, hybrid composite resin and traditional glass ionomer cement restorations of primary molars during a 6 month period. in the second pard of the study, the marginal leakage of the restorative materials; Compoglass, Dyract, TPH Spectrum and lonofil U were investigated comparatively. A total of 52 restorated primary molars were extracted after a 6 month period. Using dye penetration technique, the113 longitudinal sections were prepared from each tooth and the sections were examined under a light microscope. There was no significant difference in the marginal leakage scores of the compomer, hybrid composite resin and traditional glass ionomer restorations. in the third part of the study, the surface microhardness of the restorative materials were investigated using Vickers Hardness Tester. The samples were divided into 4 groups, each consisting of 8 specimens. Although there were no significant difference in the surface microhardness numbers of Compoglass and Dyract compomer restorative materials, the surface microhardness number of hybrid composite resin restorative material was found higher than the other restorative materials. The surface microhardness of lonofil U after 14 days was found higher than compomer restorative materials. in the fourth part of the study, the wear of the restorative materials were investigated using vvear-testing apparatus. The samples were divided into 4 groups, each consisting of 6 speciments. No significant difference were found in the vvear scores of the materials. The results of the study shovved that compomer restorative materials are capable of in the restorations of deciduous teeth.

Benzer Tezler

  1. Kompomer, cam iyonomer ve kompozit rezin dolgu maddelerinin dentine bağlanma dirençlerinin ve kenar sızıntılarının deneysel olarak araştırılması

    An in vitro investigation of the tensile band strength and microleakage of compomer, glass lonomer and composite resin restrative materials on human teeth

    YAĞMUR ŞENER

    Doktora

    Türkçe

    Türkçe

    1998

    Diş HekimliğiSelçuk Üniversitesi

    Pedodonti Ana Bilim Dalı

    DOÇ. DR. ALPARSLAN GÖKALP

  2. İki farklı kompomer retrograd dolgu maddesinin uzun dönemdeki mikrosızıntılarını sıvı filtrasyon yöntemiyle dentinle kenar uyumlarının taramalı elektron mikroskobuyla amalgamla karşılaştırmalı olarak incelenmesi

    Long-term evaluation of two compomers as a retrograde filling with a fluid filtration method and the marginal adaptation with the scanning electron microscope

    SELÇUK MECİ

    Doktora

    Türkçe

    Türkçe

    2001

    Diş Hekimliğiİstanbul Üniversitesi

    Diş Hastalıkları ve Tedavisi Ana Bilim Dalı

    PROF.DR. SEÇKİN DİNDAR

  3. Adhesive köprülerde dentin ve mine bağlantısının değerlendirilmesi

    Comparison of dentin and enamel bonding in adhesive bridges

    YASEMİN ATLI

    Doktora

    Türkçe

    Türkçe

    1998

    Diş HekimliğiGazi Üniversitesi

    Protetik Diş Tedavisi Ana Bilim Dalı

    PROF. DR. YAVUZ BURGAZ