Zirkonya alt yapılı porselen restorasyonların tamirinde endirekt faset uygulaması yöntemi ile direk tamir yönteminin bağlanma dayanımının, invitro olarak karşılaştırılması

An in vitro comparison of shear bond strength in indirect facet application method and direct repair method in zirconia-supported porcelain restorations

  1. Tez No: 671913
  2. Yazar: TUĞÇE MERVE ORDUERİ KILAVUZ
  3. Danışmanlar: PROF. DR. MEHMET MUZAFFER ATEŞ
  4. Tez Türü: Doktora
  5. Konular: Diş Hekimliği, Dentistry
  6. Anahtar Kelimeler: Dental bonding, Dental porselen, Dental restorasyon, Dental stres analizi, Zirkonyum, Dental bonding, Dental porcelain, Dental restoration, Dental stress analysis, Zirconium
  7. Yıl: 2021
  8. Dil: Türkçe
  9. Üniversite: İstanbul Medipol Üniversitesi
  10. Enstitü: Sağlık Bilimleri Enstitüsü
  11. Ana Bilim Dalı: Protetik Diş Tedavisi Ana Bilim Dalı
  12. Bilim Dalı: Belirtilmemiş.
  13. Sayfa Sayısı: Belirtilmemiş.

Özet

Bu çalışmanın amacı, zirkonya (Zr) alt yapılı restorasyonlarda karşılaşılan kırıkların, lamina veneerler ile indirekt ve kompozit sistemlerle yapılan direkt tamir yöntemlerinin bağlanma dayanımlarını karşılaştırmaktır. Çalışmada gruplar ağız içerisindeki porselen kırıklarını taklit edecek şekilde farklı porselen yüzdeleri ile oluşturuldu. Grup A = %100 Zr alan; Grup B= %70 Zr, %30 porselen alan; Grup C= %50 Zr, %50 porselen alan; Grup D= %30 Zr, %70 porselen alan; Grup E= %100 porselen alan, olmak üzere deney örnekleri hazırlandı. Grupların yarısına kompozit ile direk tamir, diğer yarısına porselen lamina veneer ile endirekt tamir yapıldı. Örnekler, yüzey işlemleri ve tamir uygulanmadan önce akrilik bloklara gömüldü. Sonrasında yüzey işlemlerini takiben, 1. gruplara lamina veneerler, 2. gruplara kompozit tamir sistemleri uygulandı. Tüm numuneler termal siklüs cihazında yaşlandırma işlemine tabii tutulduktan sonra, üniversal test cihazında bağlanma dayanımı değerlendirildi ve elde edilen veriler kayıt altına alındı. Örnekler stereomikroskop ile incelendi ve kırık tiplerine göre sınıflandırıldı (adeziv/ koheziv/ kombine). Bağlanma kuvveti verileri, bağımsız örnekler t testi ile değerlendirildi. Gruplar arasında, lamina ile yapılan tamirlerin bağlanma dayanımı, kompozit ile yapılan tamirlerden daha yüksek bulundu. İstatiksel olarak, Grup C hariç diğer bütün gruplarda endirekt tamir grupları lehine anlamlı fark bulundu. En yüksek bağlanma dayanımı Grup A da endirekt tamir yönteminde bulurken, en düşük bağlanma dayanımı Grup E de direkt tamir yönteminde bulundu. En çok adeziv kırık tipi kompozit ile tamir yapılan gruplarda görüldü.

Özet (Çeviri)

The aim of this study is to compare the bond strength of indirect repair method with laminate veneers and direct repair methods with composite systems in fractures of zirconia based porcelains. In the study, groups were formed with different porcelain percentages to imitate porcelain fractures in the mouth. The experimental samples were grouped as Group A= 100% Zr; Group B= 70% Zr, 30% porcelain surface; Group C= 50% Zr, 50% porcelain surface; Group D= 30% Zr, 70% porcelain surface; Group E= 100% porcelain surface. Half of which were repaired with composite and half of them were repaired with indirect facet method by porcelain laminate veneers. Samples were embedded in acrylic blocks before surface treatment and repair was applied. After the surface treatments, laminate veneers were applied to the 1st groups and composite repair systems to the 2nd groups. After all the samples were aged in the thermal cycle device, the bond strength was evaluated in the universal test device and the data obtained were recorded. Samples were examined with a stereomicroscope and classified according to fracture types (adhesive / cohesive / combined). Bond strength data were evaluated with independent t test statistics. Among the groups, the bond strength of repairs made with laminate veneer was higher than repairs made with composite. Statistically, there is a significant difference in favor of indirect repair groups in all groups except group C. The highest bond strength was found in the indirect repair method in group A, while the lowest bond strength was found in the direct repair method in group E. The most adhesive fracture type was seen in the composite groups.

Benzer Tezler

  1. Zirkonyum alt yapılı porselen restorasyonların tamirinde kullanılan kompozitin bağlantı direnci üzerine yüzey işlemlerinin etkisinin incelenmesi

    The effect of surface treatments on the shear bond strenght of composite material that is used in the repairment of zirconia based ceramic restorations

    DUYGU KÜRKLÜ

    Doktora

    Türkçe

    Türkçe

    2011

    Diş HekimliğiAtatürk Üniversitesi

    Protetik Diş Tedavisi Ana Bilim Dalı

    PROF. DR. NURAN YANIKOĞLU

  2. Soğuk plazma uygulamasının sabit protetik restorasyonların tamirindeki etkinliğinin incelenmesi

    Investigation of the effectiveness of non-thermal plasma application on repair of fixed prosthetic restorations

    MEHMET KÖSE

    Diş Hekimliği Uzmanlık

    Türkçe

    Türkçe

    2022

    Diş Hekimliğiİzmir Katip Çelebi Üniversitesi

    Protetik Diş Tedavisi Ana Bilim Dalı

    DR. ÖĞR. ÜYESİ ÖZLEM ÇÖLGEÇEN

  3. Fırınlama sayısının ve yaşlandırmanın zirkonyum restorasyonların rengine etkisi

    The effects of number of firings and aging on the color of the zirconium based restorations

    BİLGE BEŞİR KALAYCI

    Doktora

    Türkçe

    Türkçe

    2014

    Diş HekimliğiKaradeniz Teknik Üniversitesi

    Protetik Diş Tedavisi Ana Bilim Dalı

    PROF. DR. FUNDA BAYINDIR

  4. Zirkonyum oksit esaslı alt yapılara uygulanan farklı yüzey işlemlerinin değişik üst yapı porselenlerinin bağlanma dayanımlarına etkisinin incelenmesi

    Investigation of the effect on the shear bond strength of several veneering porcelains to zirconium oxide based substructures treated with different surface treatments

    BİLAL HOLOĞLU

    Doktora

    Türkçe

    Türkçe

    2011

    Diş HekimliğiAtatürk Üniversitesi

    Protetik Diş Tedavisi Ana Bilim Dalı

    PROF. DR. ZEYNEP YEŞİL DUYMUŞ

  5. Zirkonya ve poli-eter-keton-keton(pekk) alt yapılı farklı seramik sistemlerinin kırılma dayanımlarının karşılaştırılması

    Compari̇son of the fracture resi̇stance of all cerami̇c crowns wi̇th zi̇rconi̇a and poly-ether-kethone-kethone(pekk) framework

    ÖZGE SEÇKİN

    Diş Hekimliği Uzmanlık

    Türkçe

    Türkçe

    2019

    Diş HekimliğiNecmettin Erbakan Üniversitesi

    Protetik Diş Tedavisi Ana Bilim Dalı

    DR. ÖĞR. ÜYESİ CEYDA AKIN