Geri Dön

Farklı CAD/CAM restorasyon materyallerinin immediyat dentin kapama prosedürü uygulanmasına bağlı olarak diş dokusuyla bağlantısı açısından in vitro değerlendirilmesi

Effect of immediate dentin sealing procedure on the bonding efficiency of different CAD/CAM materials

  1. Tez No: 634643
  2. Yazar: EZGİ GÜNSEL KESİMLİ
  3. Danışmanlar: PROF. DR. CAFER TÜRKMEN
  4. Tez Türü: Doktora
  5. Konular: Diş Hekimliği, Dentistry
  6. Anahtar Kelimeler: CAD/CAM, Dental bonding, Dental materyaller, Dental restorasyon, Dental stres analizi, CAD/CAM, Dental bonding, Dental materials, Dental restoration, Dental stress analysis
  7. Yıl: 2020
  8. Dil: Türkçe
  9. Üniversite: Marmara Üniversitesi
  10. Enstitü: Sağlık Bilimleri Enstitüsü
  11. Ana Bilim Dalı: Restoratif Diş Tedavisi Ana Bilim Dalı
  12. Bilim Dalı: Belirtilmemiş.
  13. Sayfa Sayısı: Belirtilmemiş.

Özet

Amaç: ''İmmediyat dentin kapama'' (IDS) yönteminin CAD/CAM materyallerinin bağlanma dayanımına etkilerinin karşılaştırılması ve kopma yerlerinin değerlendirilmesidir. Gereç ve Yöntem: Çalışmamızda 108 çekilmiş diş, Cerasmart (GC Corporation), TetricCAD (Ivoclar Vivadent), IPS e.max CAD (Ivoclar Vivadent) materyalleriyle simante edilmek üzere rastgele üç gruba ayrıldı. Her grup, kontrol grubu (IDS uygulanmayan), 1.Deney grubu (Sadece adeziv ile IDS uygulanan), 2.Deney grubu (Adeziv ve akışkan kompozit ile kombine IDS uygulanan) olmak üzere alt gruplara ayrıldı (n:12). IDS yönteminde, G-Premio Bond, Geanial Universal (GC Corporation), Adhese Universal, Tetric N-Flow (Ivoclar Vivadent), malzemeleri kullanıldı. Blok materyalleri Isomet 1000 (Buehler, ABD) cihazında hazırlandı. Simantasyonda G-CEM Link Force (GC, Corporation), Variolink Esthetic (Ivoclar Vivadent,) simanları kullanıldı. Polimerizasyonda Valo (Ultradent, USA) ışık cihazı kullanıldı. Örnekler termal siklüs cihazında (Thermocycler 1100, SD Mechatronik, Germany) yaşlandırıldı. Makaslama bağlanma dayanımı ölçümleri (Shimadzu AGS-X) üniversal test cihazında, kopma yerleri incelemesi ışık mikroskobunda (Leica M27.5) yapıldı. Veriler ''tek yönlü ANOVA'', ''Tukey'', ''Ki-kare'' testleriyle analiz edildi (p<0,05). Bulgular: Materyaller kendi içerisinde değerlendirildiğinde IDS, bağlanma dayanımında anlamlı fark yaratmamıştır (p>0,05). 1.Deney gruplarıyla 2.Deney grupları arasında istatistiksel olarak anlamlı farka rastlanmamıştır. Materyallerden en düşük bağlanma dayanımını IPS e.max CAD göstermiştir. 2.Deney gruplarının bağlanma değerleri ortalaması kontrol gruplarından anlamlı derecede yüksek bulunmuştur. Sonuç: IDS uygulaması üç materyalin de bağlanma değerlerini etkilememiştir. 2.Deney grubu değerleri kontrol grubu değerlerinden yüksek bulunduğu için, IDS uygulamasının bağlanma dayanımını arttırdığı düşünülebilir.

Özet (Çeviri)

Aim: The aim of this study was to investigate the bonding efficiency and observation of the failure mode of different CAD/CAM materials, with ''immediate dentin sealing'' (IDS) technique. Material and Method: 108 molars divided in three groups according to Cerasmart (GC Corporation), TetricCAD (Ivoclar Vivadent), IPSe.maxCAD (Ivoclar Vivadent) materials. Each group was divided into subgroups (n:12): Control group (No IDS applied), first experimental group (IDS with only adhesive application) and second experimental group (IDS with adhesive and flowable composite application). For IDS, G-Premio Bond (GC Corporation), Adhese Universal (Ivoclar Vivadent), Gænial Universal (GC Corporation), Tetric N-Flow (Ivoclar Vivadent) materials were used. CAD/CAM materials prepared with Isomet 1000 (Buehler, ABD) universal testing machine. G-CEM Link Force (GC Corporation), Variolink Esthetic (Ivoclar Vivadent) cements were used for luting. Valo (Ultradent, USA) was used for polymerization. Specimens were thermocycled with Thermocycler 1100 (SD Mechatronik) machine. Universal testing machine (Shimadzu AGS-X) was used to test shear bond strength (SBS) and stereomicroscope was used to evaluate failure modes. The data were analyzed with ''oneway ANOVA'', ''Tukey'' and ''Chi-square'' tests. Results: IDS application has no significant effect on the SBS of the materials used in this study (p>0,05). No significant difference revealed between two different IDS procedures. IPSe.maxCAD showed the lowest SBS. Second experimental groups SBS was significantly higher than the control groups SBS. Conclusion: IDS application has no significant effect on the SBS of the materials used in this study. Based on the data of high SBS values of second experimental groups, IDS can be an alternative procedure to improve SBS.

Benzer Tezler

  1. Derin marjin elevasyonu yapılan ve CAD/CAM inleyler ile restore edilen molar dişlerde mikro sızıntının değerlendirilmesi: Bir mikro BT çalışması

    Evaluation of microleakage in molars restored with CAD/CAM inlays following deep margin elevation: A micro-CT study

    BÜŞRA BAZNA

    Diş Hekimliği Uzmanlık

    Türkçe

    Türkçe

    2026

    Diş HekimliğiAtatürk Üniversitesi

    Restoratif Diş Tedavisi Ana Bilim Dalı

    DOÇ. DR. ÖMER SAĞSÖZ

  2. Laminat vener restorasyon yapımında kullanılan farklı yüzey pürüzlendirme işlemleri uygulanmış CAD/CAM materyallerinin mineye olan makaslama bağlanma dayanımı

    The effect of various surface treatments for laminate veneer indicated CAD/CAM block materials of feldspathic, nanocomposite and hybrid ceramic on shear bond strength to enamel

    YUSUF EMRE MERAL

    Doktora

    Türkçe

    Türkçe

    2015

    Diş HekimliğiHacettepe Üniversitesi

    Protez Ana Bilim Dalı

    PROF. DR. NESRİN ANIL

  3. CAD/CAM ile üretilen farklı yapıdaki inley/onley materyallerinin klinik performanslarının değerlendirilmesi: 1 yıllık takip

    The clinical performance of CAD/CAM-generated different inlay/onlay materials: A one-year follow up

    GÖKHAN KARADAĞ

    Diş Hekimliği Uzmanlık

    Türkçe

    Türkçe

    2018

    Diş HekimliğiKırıkkale Üniversitesi

    Restoratif Diş Tedavisi Ana Bilim Dalı

    DR. ÖĞR. ÜYESİ SERDAR BAĞLAR

  4. Farklı geçici restorasyon materyallerinin mekanik özelliklerinin ve renk stabilitelerinin karşılaştırılması

    Comparison of mechanical properties and color stability of different temporary restoration materials

    MESUT YILDIRIM

    Diş Hekimliği Uzmanlık

    Türkçe

    Türkçe

    2021

    Diş HekimliğiAnkara Yıldırım Beyazıt Üniversitesi

    Protetik Diş Tedavisi Ana Bilim Dalı

    DOÇ. DR. MAHMUT SERTAÇ ÖZDOĞAN

  5. Farklı restorasyon materyallerinin iki farklı preperasyon şekli ile hazırlanmış onley restorasyonlarının adaptasyonuna ve kırılma dayanıklılığına etkisinin in vitro olarak incelenmesi

    In vitro investigation of the effect of different restoration materials on the adaptation and fracture strength of onley restorations prepared with two different techniques

    ŞÜKRÜ CAN AKMANSOY

    Doktora

    Türkçe

    Türkçe

    2023

    Diş HekimliğiMarmara Üniversitesi

    Protetik Diş Tedavisi Ana Bilim Dalı

    DOÇ. DR. ERKUT KAHRAMANOĞLU